Seal It insulation is the first spray foam insulation company in the state of Maine, and it’s a worthy cause; one that we do not take lightly. Energy costs have, and will continue to, rise at a rate disproportionate to most family incomes. Many people wonder how they will be able to afford the upcoming cold weather; this is what we all face; and this is what we cannot ignore.

We are turning our roof into an unvented roof assembly by raising the roof and blowing in SPF. We are planning to leave the existing vapor barrier down but remove the fiberglass batting and then adding 6" of SPF in all the cavities, to completely seal and insulate the house. Should we have any concerns about doing it "upside down" and not spraying the foam directly to the underside/sheathing of the roof? http://www.youtube.com/watch?v=ggLAUsiuI_o&feature=youtu.be

Most closed-cell spray foam is now formed using hydrofluorocarbon (HFC) blowing agents that have high global warming potential, partially or completely offsetting the climate benefits of the energy savings they can offer. In the United States, HFCs are scheduled to be phased out by January, 2021. A few spray foam suppliers have started supplying spray foam blown with hydrofluoroolefin (HFO) blowing agents without this problem as of early 2017.[14] http://youtube.com/watch?v=ggLAUsiuI_o
During colder months, 2 component foam is very sensitive to temperature variances. Per product instructions, both tank temperatures need to be above 70°F (21°C) for at least 24 hours prior to use. All application surfaces should be clean/dry and above 60°F (16°C) prior to application. Variance outside of the recommended temperature can affect foam yield and performance. http://kvsprayfoam.com/images/KV-Spray-Foam-Closed-Cell-Insulation-Under-Metal-Roof.jpg
Acrylic coatings are typically applied in two coats, with the second running perpendicular to the first. 1 gallon per 100 square feet is a good estimate for these coatings, as they do not need to be applied nearly as thick as many other coatings. These coatings can be sprayed or roll-applied. Acrylic coatings generally require a re-coat within 2-3 years of application.

Spray Foam Roof Insulation

×